Crushed marble aggregate versus sludge-derived powder from the same source: Comparative performance as river-sand replacements in cement mortars


Şenol A. F., Çalışkan Ö.

CONSTRUCTION AND BUILDING MATERIALS, cilt.549, ss.1-27, 2026 (SCI-Expanded, Scopus)

  • Yayın Türü: Makale / Tam Makale
  • Cilt numarası: 549
  • Basım Tarihi: 2026
  • Doi Numarası: 10.1016/j.conbuildmat.2026.148785
  • Dergi Adı: CONSTRUCTION AND BUILDING MATERIALS
  • Derginin Tarandığı İndeksler: Scopus, Science Citation Index Expanded (SCI-EXPANDED), Compendex, INSPEC
  • Sayfa Sayıları: ss.1-27
  • Bilecik Şeyh Edebali Üniversitesi Adresli: Evet

Özet

Crushed marble aggregate and sludge-derived powder differ in particle morphology, grading, and fineness, requiring these characteristics to be considered together when comparing their performance as sand replacements. This study compares crushed marble aggregate (M, 0–4 mm) and sludge-derived powder (P, <75 µm) obtained from the same marble-processing facility as partial river-sand replacements in cement mortars. M and P replaced sand at 5–30 wt% and 2.5–10 wt%, respectively, with shared levels of 5% and 10% enabling comparisons at equal replacement masses. Fresh properties, strength development, transport properties, abrasion resistance, residual performance after exposure to 400 and 800 °C, and microstructure were evaluated. At 90 days, M10 provided the highest compressive strength within the M series, 8.4% above the control, whereas M20 provided the highest flexural strength within this series. P7.5 achieved the highest flexural and compressive strengths among all mixtures, with increases of 11.3% and 12.5%, respectively, and the lowest apparent porosity, water absorption, and sorptivity. P5 exhibited the lowest abrasion loss. At 800 °C, M10 and M20 yielded the two highest residual flexural and compressive strength values, with M10 exceeding the control by 274.5% and 84.7%, respectively. XRD and FE-SEM/EDX observations provided complementary phase and microstructural information. Particle packing, mechanical interlocking, and filler-induced densification were considered possible explanations for the performance trends; their individual contributions were not quantified. The results show that the most favorable replacement level depended on the measured property and exposure condition within the investigated ranges.