The Effect of Magnetized Water on Compressive and Flexural Strength of Reactive Powder Concretes


Creative Commons License

MOHABBI M., VAROLGÜNEŞ S.

Bilecik Şeyh Edebali Üniversitesi Fen Bilimleri Dergisi, vol.6, no.1a, pp.21-29, 2019 (Peer-Reviewed Journal)

Abstract

The aim of this study is to investigate the effect of magnetized water on compressive and flexural strength of reactive powder concrete (RPC). Different magnetic field intensities can be used for magnetic water production. In this study, the effects of three different magnetic field intensities i.e. 0.8-1 and 1.2 Tesla have been assessed on compressive and flexural strength of RPC. The magnetic water used for manufacturing of the specimens was exposed to magnetic fields for 20 minutes in all mixes. When the results are assessed, it can be concluded that using of magnetic water instead of normal water causes increase in 7 and 28 days compressive and flexural strength. In addition, it has been determined that the most efficient magnetic field strength is 1 Tesla to increase the strength.
Bu çalışmanın amacı; manyetize edilmiş suyun, lifli ve lifsiz reaktif pudra betonların (RPB) basınç ve eğilmedayanımı üzerindeki etkisini incelemektir. Farklı manyetik alan şiddetleri manyetik su üretimi içinkullanılabilmektedir. Bu çalışmada; 0.8-1 ve 1.2 Tesla şiddetindeki üç farklı manyetik alan şiddeti seçilmiştir.Manyetik su üretimi için farklı manyetik alan şiddetlerinde bekletme süresi 20 dakika olarak sabit alınmıştır. Eldeedilen sonuçlar incelendiğinde; normal su kullanımı yerine manyetik su kullanımı, 7 ve 28 günlük basınç ve eğilmedayanımlarının artmasını sağladığı görülmüştür. Ayrıca manyetize edilmiş suyun, RPB’lerin basınç ve eğilmedayanımına olumlu etkisi olduğu ve dayanımı artırmak için en verimli manyetik alan şiddetinin 1 Tesla olduğu tespitedilmiştir.