Nanomechanical Characterization of Electrospun PLLA-co-PCL Vascular Grafts by Nanoindentation
ISMSIT 2017: 1st International Symposium on Multidisciplinary Studies and Innovative Technologies, 2 Kasım - 04 Aralık 2017, (Özet Bildiri)