Proceedings of the 8th Conference and Exhibition of the European Ceramic Society, İstanbul, Türkiye, 29 Haziran - 03 Temmuz 2003, cilt.264-268, ss.581-584
In this study, tribological performance of ceramic coatings (Cr 2O3, Al2O3TiO2 and ZrO2CaO) deposited on commercial poly ethyleneterephthalate have been examined by rubbing Al2O3 balls thereon. The Cr 2O3 coating exhibited the greatest hardness and wear resitance in comparison to Al2O3TiO2 and ZrO2CaO coatings. The wear resistance of the coatings increased with increasing hardness.